The sensitivity of Ni-based superalloy to hole making operations: Influence of process parameters on subsurface damage and residual stress

J. Kwong, D. A. Axinte, P. J. Withers

Research output: Journal PublicationArticlepeer-review

73 Citations (Scopus)

Fingerprint

Dive into the research topics of 'The sensitivity of Ni-based superalloy to hole making operations: Influence of process parameters on subsurface damage and residual stress'. Together they form a unique fingerprint.

Engineering & Materials Science

Chemical Compounds